Tack welders
Tack welders
(OP)
According to ASME do I need to certify my tack welders as long as all tack weld is removed by machining? If so what section/paragraph states the requirements for it? Thanks
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Tack welders
Which section of the Code is your item? Section I, Part PW does state that if a tack weld becomes part of a pressure retaining weld or structural attachment weld, the welder must be qualified but not necessarily identified.
Without knowing more about your specific application, I would tell you this that a person making ANY tack welds to pressure retaining items should be qualified AND use a qualified welding procedure.
RE: Tack welders
RE: Tack welders
No.
RE: Tack welders