carbon equivalent number
carbon equivalent number
(OP)
What exactly is the significance of carbon equivalent number calculated for a given steel from individual percentages such as MN, CR, MO, V, CU, NI etc. ?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: carbon equivalent number
RE: carbon equivalent number