INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

2TIMES PWHT FOR PN¦1 Gr.1

2TIMES PWHT FOR PN¦1 Gr.1

2TIMES PWHT FOR PN¦1 Gr.1

(OP)
Dear All
As concern the materials A 266 Cl.1 and A 350 LF1 , you are kindly asked  if according to ASME Code there are particular requirements for two times Post Weld Heat Treated materials.
Thank you for cooperation.  

RE: 2TIMES PWHT FOR PN¦1 Gr.1

The weld procedure qualification record (WPQR) should reflect the total or cumulative time for PWHT.

RE: 2TIMES PWHT FOR PN¦1 Gr.1

Please refer to ASME VIII, Div.1 UCS-85, UHT-81 & UHT-82 with regard to heat treatment requirements for base materials.

RE: 2TIMES PWHT FOR PN¦1 Gr.1

(OP)
thank you All smile

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources