INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Materials Question

Materials Question

Materials Question

(OP)
I've been hearing the term "high alloy" a lot lately, but nobody seems to be naming any specific grades of steel.  I'm a little confused by the term, not sure what kind of steel they are talking about.  Is it chromoly and high nickel steels??  Can anyone list for me common grades of "high alloy" steel used in vessel and heat exchanger design, or refer me to a website?

Thanks in advance.

RE: Materials Question

If you look in Sect 8, Div. 1, UHA then you'll know what high alloy is.

RE: Materials Question

(OP)
Yeah...right...a little on the glaringly obvious side.  Note my embarasment.  Feel free to relocate this post to the "stupid questions" forum.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources