INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Carbon fiber wheels

Carbon fiber wheels

Carbon fiber wheels

(OP)
I know there was a thread on this before, but I couldn't find it...


Now Equipped With Exclusively Designed Dymag Carbon/Magnesium Wheels

RIVIERA BEACH, FL (May 2006) Mosler Automotive today announced that its Mosler MT 900S will be the first production car to be factory-equipped with high-performance carbon fiber wheels. The specialty, ultra-lightweight rims will be designed exclusively for the Mosler and manufactured by Dymag, a leading wheel manufacturer that has been producing carbon fiber wheels for motorcycles for more than four years.

The revolutionary 18 and 20-inch nine-spoke Dymag wheels sport a magnesium center hub with carbon fiber rims and have been specially designed to complement the silhouette of the MT 900S. The Mosler's new carbon fiber front rims weigh 14 pounds, versus the 24 pounds for its current forged aluminum OZ wheels and the new Dymag carbon fiber rear rims weigh a mere 17.5 pounds each compared to 28.5 pounds each for the OZ aluminum versions. This translates into a total reduction in rotating unsprung weight (RUM) 42 pounds.

"The Dymag carbon/magnesium wheels have nearly half as much rotational inertia as forged aluminum wheels," says company founder Warren Mosler. "And, of course, pursuant to our imperative for total performance, the large savings in unsprung weight improves handling and ride qualities as well as our already extreme acceleration, braking and cornering."

The Mosler MT 900S is a 435-hp, LS6-powered, ultra-high performance two-seat, mid-engined road car, with aggressively styled bodywork and race car heritage. In third-party testing it officially set 9 performance records for acceleration, braking and handling, including an impressive 0-60mph time of 3.1 seconds. The supercar has successfully completed U.S. EPA Emission and crash testing, including DOT and California Air Resources Board (CARB) certification, and will be coming to American auto enthusiasts in the coming months.

The 50-state legal road models will be available exclusively through one of North America's premier Corvette specialist dealers, "Corvette Mike" Vietro, ( www.corvettemike.com ), whose facility in Anaheim, California heads the U.S. distribution and sales efforts for the $189,900 Mosler MT 900S. For additional information on Mosler Automotive, the Mosler MT 900S or its European racing schedule, visit www.moslerauto.com.

-Dave
Everything should be designed as simple as possible, but not simpler.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources