May i know the differnce between sintering and drying
Thanks
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: DRYING
Sintering is a process in which atomic diffusion is activated by heating to a temperature that is a significant fraction of the melting temperature. For many materials, this can be above 1000 °C, so the temperature differences between drying and sintering are enormous.
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
RE: DRYING
Evaporation and transpiration commonly occur at temperatures well below boiling. Common examples are clothes driers, hair driers and hand driers. Many industrial drying processes occur below boiling.
Sublimation - by definition - occurs below the freezing point.
RE: DRYING
Yes, point well taken. My point was one of magnitude orders: 102 vs. 103.
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
RE: DRYING
I work in the investment casting industry so I have some background in the drying of ceramics. First off, let me give you a good reference that explains the theory behind drying:
"Theory of Drying". Journal of the American Ceramic Society. Vol - 73. Pages 3-14. 1990 by Gearge W Scherer.
Drying and sintering aren’t the same but in most cases they are used in succession. In the process of drying water evaporates from the surface. The surface tension between the liquid and solid phase causes a contraction in the solid network (more eloquently called a gel). This contraction forms van der waals bonds between the solids. This is why the network stiffens. Sintering would be the next step. Pressure/heat is applied to the solid network. The individual grains bond together. This description of sintering is an oversimplification but more detail would require too much writing. I hope this helps.
Regards,
Matlsguy