INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Piping A672 Gr C65 Cl22 Overlay Cladding

Piping A672 Gr C65 Cl22 Overlay Cladding

Piping A672 Gr C65 Cl22 Overlay Cladding

(OP)
Colleagues,

By following:

B31.3, 323.4.3, d) to

ASME VIII Div 1, UCL 34, a) to

ASME VIII Div 1, Table UCS-56, Note c) 5)

May I conclude that, if an A672 GrC65 Cl22 pipe up to 32 mm wall thickness is clad by overlay welding, then it does not require another PWHT?
 

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

RE: Piping A672 Gr C65 Cl22 Overlay Cladding

Yes.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources