BS 4871 pt 1
BS 4871 pt 1
(OP)
Can anybody tell me in Bs 4871 pt 1 when I get Charpy's done for the welders test piece do I have to take the samples from FL,FL+2,FL=5 AND HAZ.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: BS 4871 pt 1
RE: BS 4871 pt 1
There is/was no requirement for mechanical testing of welders test pieces, only for weld procedure qualification, which is covered by EN ISO 15614-1:2004.
This details test pieces , locations of test samples and the conditions under which impact tests are required. You need to get hold of copies of these standards.
RE: BS 4871 pt 1