Iron, Zinc & Sulfur ternary phase diagram data
Iron, Zinc & Sulfur ternary phase diagram data
(OP)
Does anybody have such a phase diagram? How 'bout zinc + sulfur binary phase diagram? My copy of the Metals Handbook does not have either and I'm looking for temperatures for when things turn to liquid.





RE: Iron, Zinc & Sulfur ternary phase diagram data
http://w
Journal of Phase Equilibria & Diffusion, Volume 25, Number 4, August 2004, pp. 382-383(2)
Vita sine litteris mors est.
RE: Iron, Zinc & Sulfur ternary phase diagram data
RE: Iron, Zinc & Sulfur ternary phase diagram data
Thomas J. Langill, Ph.D., Technical Director
tlangill@galvanizeit.org x14
Phone: 720.554.0900
Fax: 720.554.0909
Address:
American Galvanizers Association
6881 South Holly Circle, Suite 108
Centennial, Colorado 80112
http://www.galvanizeit.org/
Vita sine litteris mors est.
RE: Iron, Zinc & Sulfur ternary phase diagram data
http://www.lindahall.org/
Check with your library and we if they have access to Metadex.