INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Coefficient of Friction - Steel & Concrete??
3

Coefficient of Friction - Steel & Concrete??

Coefficient of Friction - Steel & Concrete??

(OP)
I can't seem to find any resources or charts on the coefficient of friction of concrete and steel together on both wet and dry surfaces.  Also, on various surfaces such as open and sealed concrete.  Is there such a thing?

RE: Coefficient of Friction - Steel & Concrete??

What you are looking for is easily tested.  Use a modification of the ASTM standard for Static Coefficient of Friction, using a steel plate pulled against a concrete surface.  You can then test the site specific condition.

RE: Coefficient of Friction - Steel & Concrete??

(OP)
Thank you Ron and DRW75 for these very useful pieces of information.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources