INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

TMS-80 Forged steel wheel

TMS-80 Forged steel wheel

TMS-80 Forged steel wheel

(OP)
Hello.  Can anyone provide any information about TMS-80 steel?  We have to provide some parts for a machine from some old drawings, and one of the parts is specified as TMS-80 forged steel wheels.  Can anyone point me in the direction of the material properties for this steel?  Also, does anyone know of any suppliers US or (preferably) Europe based who might be able to either provide these off the shelf, or who could manufacture them.  Thanks.

RE: TMS-80 Forged steel wheel

Found this information on Google;
Timken introduces TMS 80™ non-. heat-treatable microalloy steel.

http://www.timken.com/

RE: TMS-80 Forged steel wheel

"TMS-80" is the old nomenclature.  These micro-alloy steels are now sold under the "MicroTec" name by Timken.  I believe the "80" refers to typical yield strength after controlled cooling from the forging temperature.  I don't have my Timken book with me but their website should have general information on the Microtec series.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources