API5LX52 equivalent material
API5LX52 equivalent material
(OP)
Hello Every body,
What are the equivalent ASTM materials to API5LX52 ?
Thank you
What are the equivalent ASTM materials to API5LX52 ?
Thank you
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
API5LX52 equivalent material
|
RE: API5LX52 equivalent material
SMYS = 52kpsi
SMTS = 60kpsi
RE: API5LX52 equivalent material
my mistake sorry :)