THPS and stainless steel
THPS and stainless steel
(OP)
Hi everybody. Is there anybody who has infos regarding possible problems of compatibility between AISI316L and THPS (Tetrakis (hydroxymethyl)phosphonium sulfate) biocide agent at commercial concentrations (that is before being injected into the water circuit)?
Thanks in advance
Thanks in advance





RE: THPS and stainless steel
Let's see, not Cl of F so no alarm bells yet.
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm
RE: THPS and stainless steel
Concentration of THPS = 50%