Performance of Galvanized Steel under High Pressure Washing
Performance of Galvanized Steel under High Pressure Washing
(OP)
Anyone have any info on the effect of high pressure washing at about 300 psi on galvanized coating? Will high pressure washing remove the galvanizing?





RE: Performance of Galvanized Steel under High Pressure Washing
I would not expect any problem with galvanizing that was done correctly, sans flaky, or large inclusions, such as ash or dross.
Vita sine litteris mors est.