limited maximum yield strength
limited maximum yield strength
(OP)
Hi
Anybody knows proper plate mill maker who could supply plate as following specification .
"" Carbon and low alloy steels shall be limited to a maximum yield strenth (Re) of 355 Mpa and maximum ultimate tensile strength (Rm) of 620 Mpa ""
Plate supplier could guarantee 430 Mpa ,Maximum Yield strenth but client stick to the value 355 Mpa without any exception .
The material to be used for Job is SA516-70.( 14t* 5 sheets * T/L 8 ton.)
Anybody knows proper plate mill maker who could supply plate as following specification .
"" Carbon and low alloy steels shall be limited to a maximum yield strenth (Re) of 355 Mpa and maximum ultimate tensile strength (Rm) of 620 Mpa ""
Plate supplier could guarantee 430 Mpa ,Maximum Yield strenth but client stick to the value 355 Mpa without any exception .
The material to be used for Job is SA516-70.( 14t* 5 sheets * T/L 8 ton.)