CS Large size Pipes Backfill material
CS Large size Pipes Backfill material
(OP)
I try to find some tips for backfill material surrounding Carbone steel pipes PN10 size from 800 to 3000 mm Dia coated with 2000 micron solvent free polyurethane





RE: CS Large size Pipes Backfill material