Valve Internals
Valve Internals
(OP)
Hi,
Anybody having experience in selecting trim materials for Ball Valves? Specified was 17-4PH for Ball Valves in a non sour hydrocarbon gas application (high pressure class 2500#).
Fabricator have valves assembled with F6 internals (13% Cr.)
As far as we know is 17-4PH a better material with respect to corrosion as well as strength.
Any recommendations/suggestions would be more than welcome and of course very much appreciated.
Thanks in advance.
Regards,
FKE
Anybody having experience in selecting trim materials for Ball Valves? Specified was 17-4PH for Ball Valves in a non sour hydrocarbon gas application (high pressure class 2500#).
Fabricator have valves assembled with F6 internals (13% Cr.)
As far as we know is 17-4PH a better material with respect to corrosion as well as strength.
Any recommendations/suggestions would be more than welcome and of course very much appreciated.
Thanks in advance.
Regards,
FKE





RE: Valve Internals
RE: Valve Internals
RE: Valve Internals
also take a look at "Valve Engineering Forum" within this site: forum408.
Hope this helps, 'NGL