INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Material Specs For AL2023

Material Specs For AL2023

Material Specs For AL2023

(OP)
Hi all,

Does anyone of you have heard of Aluminum Alloy 2023? If so, could you provide me the material specifications as well as the vendor whom I and reach to buy?

Thanks!

RE: Material Specs For AL2023

I checked the Aluminum Association registered alloys list for 2004 and no 2023 alloy is listed.

RE: Material Specs For AL2023

No mention of Al 2023 in the following references:
Aluminum, vols. I, II & III (1967),
ASM Handbook vol. 2, 9th Edn. (1979),
Aluminum: Properties and Physical Metallurgy (1984),
Smithells Metals Reference Book, 7th Edn. (1992),
Handbook of Materials for Product Selection, 3rd Edn.; the 178-page chapter "Aluminum" covers Aluminum Association & ASTM specs. (2001),
Light Alloys, 4th Edn. (2006),
www.astm.org
www.matweb.com

I found limited supplies from an Internet search:
Pipe and tube fittings for handrails, with mill, satin and anodized finishes:
http://www.geobezdan.com/geobezdan/index.jsp?cid=321&sid=-20-750-3211

Aluminum 2023-T351 Hexagons, sizes 8' to 12' lengths, 1/4" to 3"
http://www.hagertysteel.com/products/aluminum.html

Due to the lack of data and availability, cannot possibly recommend for any critical use, especially not aerospace.   

RE: Material Specs For AL2023

I couldn't find it in Mil handbook 5, ASM Handbook vol 4 (heat treatment), PWA manual, T.O. 1-1A-9, or any of the filler rod guides we have here at Edwards either.  2008, 2024, and 2219 sure, but no 2023.

sorry,

Kalroy

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources