Shear strength of EN24T (817M40T)
Shear strength of EN24T (817M40T)
(OP)
Any one have a reference source for the shear strength of EN24T or EN16T?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Shear strength of EN24T (817M40T)
|
Shear strength of EN24T (817M40T)Shear strength of EN24T (817M40T)(OP)
Any one have a reference source for the shear strength of EN24T or EN16T?
Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesWhat is rapid injection molding? For engineers working with tight product design timelines, rapid injection molding can be a critical tool for prototyping and testing functional models. Download Now
The world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
|
RE: Shear strength of EN24T (817M40T)
Yield 98560 psi min
Ultimate 123200 - 145600 psi.
Perhaps someone can suggest a reasonable relationship between this data and shear properties.
RE: Shear strength of EN24T (817M40T)
0.75 * Ultimate tensile strength
RE: Shear strength of EN24T (817M40T)
Most of the data I have seen for shear strength is ~ 0.6 times the ultimate tensile stress.
thread725-32814
thread404-83055
Actual data can be found for many materials in AR-MMPDS-01 or MIL-HDBK-5:
http://www
http://assist.daps.dla.mil/quicksearch/
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
RE: Shear strength of EN24T (817M40T)
regards
John