INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stainless steel casting for high temperature SO2/CO2 environment.

Stainless steel casting for high temperature SO2/CO2 environment.

Stainless steel casting for high temperature SO2/CO2 environment.

(OP)
I have just received a mail mentioning that furnace liners casting grade HK for copper smelter are failing early. Please suggest if anyone has any experience in this area. Will be most grateful for any assistance.

RE: Stainless steel casting for high temperature SO2/CO2 environment.

(OP)
C 0,4-0,6; Cr 35-37; Ni 45-48; Si 1-2; Nb 0,8-1,2; Mo 0,5-0,8; Ti 0,5-0,8;

This is the alloy which my good friends from AFE Klefisch have recommended.

The cost is going to be prohibitive I suppose for replacement

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources