In qualifying a PQR to ASME Sec IX, QW 181, where testing will be to QW 183, with no mechanical tests involved, is PWHT an essential variable?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Fillet Weld Procedure, P4 - P7
|
RE: Fillet Weld Procedure, P4 - P7
If you intend to qualify a fillet weld WPS in a situation where PWHT is required by Code for fillet welds, yes, PWHT should be included as an essential welding variable for this procedure.