INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Inconel Material specifications

Inconel Material specifications

Inconel Material specifications

(OP)
Can someone give me the standard SA inconel specifications for Section II for a Section VIII, Div.1 vessel?
Pipe, plate, forging?

Thanks.

RE: Inconel Material specifications

Yes. However, rather than citing specific ASME SBS Material Specifications, I have included the comprehensive web site from Special Metals. Find the alloy of interest in their alloy portfolio, open the pdf file of the alloy, and at the end of the Technical Bulletin you will find an ASME SB Specification in either plate, sheet or other product form.

http://www.specialmetals.com/

RE: Inconel Material specifications

(OP)
Thanks metengr.  That website is full of technical info.  One of the best I've seen.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources