INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Coperion MEGAcompounder Gearbox foaming Problem

Coperion MEGAcompounder Gearbox foaming Problem

Coperion MEGAcompounder Gearbox foaming Problem

(OP)
We got a ZSK-70 Megacompounder loaded with Castrol 1715-320 semi-synthetic, it's at 120°F running 50PSI spray gearbox. We get foaming from the top at start up, and from the sample port 1" from the bottom of the tank, theres entrainment. Some think a switch to a full synthetic oil will do the trick, I'm not so sure. We did an ultra sound for leaks, and found some, they got permatex'ed, there's no line restrictions or resistance, no turbulance or shock wave, no external forces. The problem I have nagging me is the temp of the oil, and a feeling of unforeseen cavitation, for the life of me, I can't figure out where. Some feel that the entrainment is do'able since it's a spray box anyways, but I want them to tell me that after the 2nd or 3rd oil change. Any help on the "unforseen" is something, really.
Thanks
db.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources