INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stainless Steel question

Stainless Steel question

Stainless Steel question

(OP)
I need to know what 1Cr18Ni9 is.  Is it 304 Stainless Steel?  Also, what is 40Cr, and QT500-7?  I think the QT500-7 is some kind of Bronze or something.  Any help would be great.
Thanks.

RE: Stainless Steel question

1Cr18Ni9 is China Standard GB1220 equivalent tp 302 Stainless Steel. A cross-listing of Chinese & international equivalent SS's is at
http://nhyh.com/en/productsteelhao.asp

40Cr is a Chinese high strength steel used in oil well drill pipe. Looks like "40" is 0.40 wt% C, "Cr" ~ 1 wt% Cr.
40Cr composition:
0.40 C, 0.95 Cr, 0.65 Mn, 0.18 Ni, 0.27 Si, 0.01 P, 0.01 S (Fe balance).


QT500-7 seems to be a Chinese performance standard for nodular cast iron:
"Continuous Cast SG Ductile Iron Bar
QT500-7
ASTM A536-84 65-45-12 / 80-55-06 / 100-70-02
JIS FC D45
DIN 1693 GGG40
BS 2789 SNG 27/12"
from http://www.dhcasting.com/continuous_cast_iron_bar.asp

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources