INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

DRILLING CPM 10V

DRILLING CPM 10V

DRILLING CPM 10V

(OP)
HI TO ALL DRILLING EXPERTS
DOES ANYONE HAVE ANY IDEA'S ON HOW TO DRILL THIS MATERIAL CPM 10V.
BRINELL HARDNESS 255/270
RUN ON A CNC LATHE WITH A BAR FEEDER
DRILL SIZES 9/64 .375 DEEP - 3/16 DRILL .250 DEEP
ALSO REAM .152 LENGTH OF REAMER .125
THANKS TO ALL IN ADVANCE

RE: DRILLING CPM 10V

You may try contacting the material distributor or any local major tooling manufacturer representitive. They should fall all over themselves to help you out. My preference is Carboloy. You can see them here:


http://www.carboloy.com/
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources