INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Hydrotest water quality of boiler

Hydrotest water quality of boiler

Hydrotest water quality of boiler

(OP)
Hi All,

Our boiler is 44barg/274C/160t/h steam production is going to get hydrotest,I want to Max. chloride content of water for hydrotest.

Thank you.

RE: Hydrotest water quality of boiler

For a boiler of this size, less than 500 ppm of chlorides should be acceptable for a boiler hydrotest followed by a thorough boiler rinse cycle, and dry lay-up.

RE: Hydrotest water quality of boiler

Hi,
I want to know that, in ASME section IX anywhere mentioned that Authorised inspector require during qualify the welder?
Also if A.I reject welder coupan, what we can do?
pls. help me asap

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources