Yield strength
Yield strength
(OP)
Do anyone know the yield strength for "AMS 5344 17-4PH", "C.S SA-36" and "St 1550" at temp. 20 and 100 20degrees Celsius?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Yield strength
0,2% Yield stress
at 100°C
>= 880 N/mm²
at 150°C
>= 830 N/mm²
at 200°C
>= 800 N/mm²
at 250°C
>= 770 N/mm²
at 300°C
>= 750 N/mm²
This is from Stahlschlussel. Please provide more information about the other steels.
RE: Yield strength
You need a starting point.
= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.
Manage it or it will manage you.
http://www.trent-tube.com/contact/Tech_Assist.cfm
RE: Yield strength