INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

GG-26CR

GG-26CR

(OP)
Can anyone tell me what the CR stands for on the old DIN GG-26 gray iron specification?  

RE: GG-26CR

A Google search indicates that it is an alloy cast iron for wear resistance contaning Cr + Mo. The % of contents and mechanical properties I am unable to get. The application mentioned is for a die part and a wear pin

RE: GG-26CR

it is %26-30 Cr and %1 Mo it is hard as cast and not mashiable it is used for parts under sever abrasion and errosion for example salary pumps and grinding balls there is standard ASTM A532  for these types

RE: GG-26CR

feraidoon,
please give me the reference for the grade. My literature search indicates that it is a machinable grade and the alloy contents are in the low range.

I am familiar with ASTM 532,. Thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources