Could anybody help me out by advising whether there is a correlation (or a rule of thumb) between cutting tool HB vs. parent metal HB or not ?
We are currently buying a gear in China and the vendor reported that the Hobbing cutting tool is wearing - out prematurely. We then asked for the HB of the tool and it was reported 300 HB. That surprised us , because :
a) It seems to be too low of a hardness for high speed steel.
b) That`s the hardness of the gear thus, a 300 HB - cutting tool will never be able to rough cut the teeth of that gear.
Any comment would be very welcome.
Thank you.
Could anybody help me out by advising whether there is a correlation (or a rule of thumb) between cutting tool HB vs. parent metal HB or not ?
We are currently buying a gear in China and the vendor reported that the Hobbing cutting tool is wearing - out prematurely. We then asked for the HB of the tool and it was reported 300 HB. That surprised us , because :
a) It seems to be too low of a hardness for high speed steel.
b) That`s the hardness of the gear thus, a 300 HB - cutting tool will never be able to rough cut the teeth of that gear.
Any comment would be very welcome.
Thank you.





RE: CUTTING TOOL HARDNESS VS. PARENT METAL HARDNESS