INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Ti-6Al-4V BLEED AIR DUCT

Ti-6Al-4V BLEED AIR DUCT

Ti-6Al-4V BLEED AIR DUCT

(OP)
I AM WORKING ON Ti-6Al-4V BLEED AIR DUCT REPAIRMENT BUT I DON`T HAVE ANY CMM OR ANY MANUALS.AFTER REPAIR I WILL HAVE TO PERFORM HYDRAUSTATIC PRESSURE TEST.

IS ANYONE OUTHERE WHO CAN HELP ME PROVIDING FORMULA SOTHAT I CAN CALCULATE PRESUURE BEFORE SETTING TEST PROCEDURE?

RE: Ti-6Al-4V BLEED AIR DUCT

The aircraft OHM, chapter 36, should cover all repairs on bleed air ducts to include hydrostatic testing. My aircraft does not have any titanium ducts and each duct installed in the aircraft is covered by part number/material spec, but I would think the data you are looking for is readily available.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources