INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

minimum temperature of A106 piping

minimum temperature of A106 piping

minimum temperature of A106 piping

(OP)
Table 323.2.2A in B31.3 shows that A106 CS Pipe minimum temp to -20F is only good to a certain wall thickness. As the wall thickness increases the allowable temp gets warmer.
Is this dependant on coincidental pressure and can deviations be allowed for short periods of time.

RE: minimum temperature of A106 piping

Your answer lies in the provisions of clause 323.2.2.  Work your scenario through and see what drops out.

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources