A sign has been specified to manufactured in HDPE, can this be manufactured in one piece with multiple colours or does it have to be individual and mechanically joined?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
HDPE Manufacturing in colour
|
HDPE Manufacturing in colourHDPE Manufacturing in colour(OP)
A sign has been specified to manufactured in HDPE, can this be manufactured in one piece with multiple colours or does it have to be individual and mechanically joined?
Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesWhat is rapid injection molding? For engineers working with tight product design timelines, rapid injection molding can be a critical tool for prototyping and testing functional models. Download Now
The world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
|
RE: HDPE Manufacturing in colour
Multi colour HDPE can be done by co extrusion, twin barrel injection or lamination.