Does anybody have any reference to a source for viscoelastic properties of babbitt metals in the temperature range 80 - 150C?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Viscoelastic properties of babbitt
|
RE: Viscoelastic properties of babbitt
The web site below is a copy of a lecture that contains a section on Babbit metals with room and elevated temperature properties. Iit might help to you;