INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Bending stress of plain concrete masonry

Bending stress of plain concrete masonry

Bending stress of plain concrete masonry

(OP)
what is the allowable bending stress of plain concrete masonry wall

RE: Bending stress of plain concrete masonry

It depends on a lot of things--type of mortar, if it is fully grouted, if it is partially grouted, and if it is  ungrouted.  Give us some more information.

DaveAtkins

RE: Bending stress of plain concrete masonry

It also depends on whether the wall spans vertically (= bending stress perp to the bed joints) or horizontally (= bending stress parallel to bed joints).




Regards,

chichuck

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources