Unknown material - 23 90 95
Unknown material - 23 90 95
(OP)
Could anyone please help me find the material specification of this material 23 90 95, this number is all I have, I think it is a high alloy steel, but I need more information.
Thanks for any help
Dustymiller
Thanks for any help
Dustymiller





RE: Unknown material - 23 90 95
RE: Unknown material - 23 90 95
Thanks for your speedy reply, I do not know what the material is to be used for as I work for a job shop and all I am doing is machining it.
Thanks
Dustymiller
RE: Unknown material - 23 90 95
I found that this is some Schwedish mark with chemical analyse : C - 0,2%; Cr - 12% Mo - 1%; Ni-0,5%; V - 0,5%
See: www.rapporte.varmeforsk.se