Tempered Glass- E value, and tensile strength??
Tempered Glass- E value, and tensile strength??
(OP)
Hi,
I want to design a tempered glass shelf and I need to know the elastic section modulus, and the allowable tensile strength.
Any help would be greatly apreciated
td





RE: Tempered Glass- E value, and tensile strength??
i foulnd these through google:
"E" for Most glass seems to be of the order of 10000ksi
The ultimate tensile stress of fully tempered glass is 24ksi, while "regular" glass is of the order of 10ksi.