INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

plexi glass structural properties

plexi glass structural properties

plexi glass structural properties

(OP)
Does anyone have info on the structural properties of plexi glass?

much apreciated

RE: plexi glass structural properties

You should contact the manufacturer. They would probablly have the best data.

Wes C.

RE: plexi glass structural properties

(OP)
Thanks wes616, but I don't know of any manufacturer. The design will be done before a mfr is chosen.

RE: plexi glass structural properties

I also recommend you contact the manufacturer.  If you don't have one chosen, dig in the phone book or the net and call around to a couple.  It might be on the net somewhere anyway, have you "Googled" it?

RE: plexi glass structural properties

(OP)
I've googled it and managed to get a few results:
bending stress of 11 ksi,and a youngs modulus of 450ksi.

I've also contacted a few manufacturers, but no replies.

RE: plexi glass structural properties

If you sound interested in a product, any sales rep should jump all over to get you the information you need.

Those values sound good to me...

Generic Values for Acrylic are

Sut = 10Ksi

Suc = 18Ksi

Wes C.
------------------------------
There are no engineers in the hottest parts of hell, because the existence of a 'hottest part' implies a temperature difference, and any marginally competent engineer would immediately use this to run a heat engine and make some other part of hell comfortably cool.  This is obviously impossible.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources