INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

The strain hardening

The strain hardening

The strain hardening

(OP)
I would like to know the strain hardening of the crane runway girder. The material of the crane runway girder is acid-proof steel. I know that the ultimate stress correlate with the hardness of the material. Does anybody know is it possible to determine the strain hardening by measure the hardness of the surface?

I hope you understand what I mean. My mother tongue is not English…

RE: The strain hardening

What is the specific material of construction used for the girder?
 

RE: The strain hardening

(OP)
The material is acid-proof steel 1.4432 / SS2343 / 316L (depending on the standard used).

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources