Coating requirment please explain how this materail is applied and to what extent does it affect the dimensional requirements of machined part after application. Is it necessary to make allowance for coating?





RE: MIL-M-3171 COATING
RE: MIL-M-3171 [now: AMS-M-3171] coating... which "Type"???
Regards, Wil Taylor
RE: MIL-M-3171 COATING
RE: MIL-M-3171 COATING
REF Ty VI: as with most chem films, there is virtually NO measureable thickness +/- change. There will probably be an increased thickness of +0.0001-inch (+0.0025-mm)... if it could be measured (I doubt if conventional measurement instruments would see any difference).