Short of testing, is it possible to assign an allowable or nominal shear strength to a mix specified to have a 28 day comp. strength of 300 (yes, three hundred)psi? Do the normal formulas apply, wherein the allowable is ~20psi? The submitted mix per yard is:
100# Type I/II
300# Grancem
2300# sand
35 gal H20
Air Entrainment