INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

incolloy 800H
5

incolloy 800H

incolloy 800H

(OP)
Does anyone know a supplier of incolloy 800H tubes (10"x12.7mm - seamless)? Any info much appreciated.

RE: incolloy 800H

try the trade name for inconel alloys  who owns the name,
so they will know who they licence it to.
er
 

RE: incolloy 800H

Seamless alloy 800H pipes are to my knowledge only available up to 8 inch. Above 8 they are welded.

RE: incolloy 800H

(OP)
thank you to all, guys. It seems that ijzer is right about the max dimensions. Nevertheless, I am astonished by this imperative request for seamless tube. As long as a welded tube would be manufactured in strict accordance to ASME rules, I don't see any problem. Any ideas?

RE: incolloy 800H

(OP)
Just for info: TPS Technitube seems to be able to supply it

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources