INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

sheet and plate

sheet and plate

sheet and plate

(OP)
What is the difference between sheet and plate?

Example:
ASME SEC II B SB-171 Specification for Copper-Alloy Plate and Sheet for Pressure Vessels, Condensers, and Heat Exchangers

RE: sheet and plate

ASME definition:

Plate: 3/16" and over thk and over 10" wide.

Sheet: under 3/16" thk and 24" and over wide.

RE: sheet and plate

(OP)
I also looked it up. SB-171 spec gives plate as 3/16" and over thk and over 12" wide not 10".

RE: sheet and plate

Sorry!!!

RE: sheet and plate

A sheet goes on your bed.

A plate goes on your table.

;)

Brian

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources