I am looking for a company that can formulate concrete for a specific use. We make concrete counter tops. We buy 5 gallon buckets and bags of concrete (I have no idea what kind it is.)then add the additives (that stink like you know what and has a lot of fibers) into the bucket with the concrete in it. Mix and pour. We are able to take it out of the mold in 24 hours and polish in 48. I am looking for a company who can make something like this for me. We want to start pouring slabs that are 70X110 and 1 1/4 thick. I have not tried this mix to see if it will hold up but we will be using a lot of this stuff shortly and need soemone to formulate it for me.
Who do I go to, to get this done?
I am in Annapolis Maryland