INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Magnetic properties of Hastelloy C276

Magnetic properties of Hastelloy C276

Magnetic properties of Hastelloy C276

(OP)
I'm having trouble finding information regarding the magnetic properties of Hastelloy C276.  Anybody know where I can look to find it?  Thanks for any help.

RE: Magnetic properties of Hastelloy C276

Try the cabot corporation

Thomas J. Walz
Carbide Processors, Inc.
www.carbideprocessor.com

RE: Magnetic properties of Hastelloy C276

Per Special Metals:
Permeability at 200 Oersted (15.9 kA/m.....1.0002

RE: Magnetic properties of Hastelloy C276

Haynes International is the producer of Hastelloy C 276, and they have a great deal of technical information available from their website:

http://www.haynesintl.com/mini/C276s/C276.htm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources