Mechanical Properties of 6105-T5
Mechanical Properties of 6105-T5
(OP)
I've been unable to find any tensile and yield strength listed for this alloy and temper of aluminum.
can anyone point me in the right direction?????
can anyone point me in the right direction?????





RE: Mechanical Properties of 6105-T5
For extruded wire, bar, rod, or shapes:
6105-T5 -- for dia up thru 12.70mm; Min UTS: 262MPa Yeild: 241 MPa ; min elong: 10%.
RE: Mechanical Properties of 6105-T5
RE: Mechanical Properties of 6105-T5