INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Chemical Resistance of Perspex

Chemical Resistance of Perspex

Chemical Resistance of Perspex

(OP)
Hi all,
I'm looking for chemical resistance information for Perspex.
Working condition I have to inquire is for water and NaOH 5% at temperature up to 60 °C

Thank you very much on advance.

RE: Chemical Resistance of Perspex

Hi Shmulik,

A search on Google for "PMMA chemical resistance" gave over 39,000 hits - should be something there for you.

If not, try one of the many manufacturers.

Rgds

Harry

RE: Chemical Resistance of Perspex

If you need a transparent thermoplastic with good chemical resistance then I suggest you try SAN instead of Perspex (tradename for PMMA). SAN varies in chemical resistance and grades with higher acrylonitrile content are better in this regard. The manufacturers can advise you on that.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources