High temperature alloys
High temperature alloys
(OP)
I need to differentiate between 'Hatelloy C' and 'Hastelloy C'. Would appreciate all the assistance I can get.
Thanks.
langahl@netscape.net
Thanks.
langahl@netscape.net
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: High temperature alloys
You have fallen victim to a typo. "Woldman's Engineering Alloys" has no listing for Hatealloy C, nor have I seen or heard of such a material in 25 years of PV design.