Methods/technologies for cleaning of moulding tools ?
Methods/technologies for cleaning of moulding tools ?
(OP)
Dear members,
I am concerned about some issues related to injection moulding of rubber. I mean surface appearance and mould cleaning from time to time.
Usually, how many cicles does a injection mould stands assuring a good surface finish of the products?
What kind of methods/technologies are commonly applied for cleaning of moulding tools?
Many thanks
Bipp
I am concerned about some issues related to injection moulding of rubber. I mean surface appearance and mould cleaning from time to time.
Usually, how many cicles does a injection mould stands assuring a good surface finish of the products?
What kind of methods/technologies are commonly applied for cleaning of moulding tools?
Many thanks
Bipp





RE: Methods/technologies for cleaning of moulding tools ?
The most common ways to clean a mold are grit blasting the cold mold with plastic grit (to reduce damage to original surface), chemical/solvent cleaning (cold mold), and by blasting the hot mold in the press with crystalized CO2 pellets.
RE: Methods/technologies for cleaning of moulding tools ?
We produce a tool that can be used to clean injection molds. It is a Plasma Pen. The pen is portable and can be used where ever you have a source of compressed air. It cleans using gas plasma and gets rid of all of the organic materials.
Please see our website www.pvateplaamerica.com for additional information. I'd also be glad to answer any questions you may have regarding this.