Our customer wants to change tin based white metal to lead based white metal for his 100 MW Hydro generator bearings. What will be the repercussions ? Where can I find info on these bearing metal compositions ?
Thx in advance.
Thx in advance.





RE: White metal bearing composition
The lead based Babbitt Metals have lower strength than the tin base so the load carrying capacity is reduced.