RE: New Concrete
The material may cost more, but the number and size of beams may come down, along with lower cranes needed and lighter trucking to the site. Also, lower footings. I would think all these would need time to develop and if it doesn't end up being competitive with current methods, it goes away.
RE: New Concrete
Here's some extra info on UHPC.
http://
RE: New Concrete
More again
http://www.tfhrc.gov/focus/nov04/01.htm